Description: 325 mesh Dolomite, CaMg(CO3)2
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 30.42% | 0.50 | |
| MgO | 21.85% | 0.50 | |
| Fe2O3 | 0.30% | - | |
| LOI | 47.40% | n/a | |
| Oxide Weight | 48.48 | ||
| Formula Weight | 92.16 | ||
Produced in Canaan, CT. A pulverized dolomitic limestone (calcium-magnesium carbonate). Used in many industries (for applications like putties, rubber, cement, plastics, ceramics, coatings).
The 40-13 designation means the largest particle size is 40 microns (325 mesh) and the oil absorption is 13 grams/100 grams.
This is attractive for dolomite clay bodies, since its fine particle size assures that there will be no problems with decrepitation that occurs with larger limestone particles.
This material is 55% CaCO3 and 43% MgCO3, 0.3% Fe2O3.
Specific gravity: 2.8
Bulk density: 1.04 g/cc (65 lbs/cubic ft)

This picture has its own page with more detail, click here to see it.
| Minerals |
Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO |
| Minerals |
Tremolite
A fiberous magnesium silicate mineral. |
| Materials |
Dolowhite
|
| Materials |
Dolomite
An inexpensive source of MgO and CaO for ceramic glazes, also a highly refractory material when fired in the absence of reactant fluxes. |
| Materials |
Camadil 95 Dolomite
|
| URLs |
https://www.mineralstech.com/business-segments/specialty-minerals/smi-sds
Dolocron 40-13 SDS This is the general page for all their products, this is in the "Ground Calcium Carbonate" section. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk