03DSFF - Cone 03 Fast Fire
04DSDH - Low Temperature Drop-and-Hold
BQ1000 - Plainsman Electric Bisque Firing Schedule
BRTF05 - Bartlett Fast Glaze Cone 05
BRTF6 - Bartlett Fast Glaze Cone 6
BRTS6 - Bartlett Slow Glaze Cone 6
BTFB04 - Bartlett Fast Bisque Cone 04
BTSB04 - Bartlett Slow Bisque Cone 04
BTSG05 - Bartlett Slow Glaze Cone 05
C04PLTP - Plainsman Low Temperature Drop-and-hold
C10RPL - Plainsman Cone 10R Firing
C5DHSC - Plainsman Cone 5 Drop-and-Hold Slow-Cool
C6DHSC - Plainsman Cone 6 Drop-and-hold, Slow Cool
C6IRED - Cone 6 Iron Reds
C6MSGL1 - Mastering Glazes Cone 6
C6PLST - Plainsman Cone 6 Electric Standard
FSCG1 - Shimbo Crystal Schedule 1
FSCGB1 - Shimbo Crystal Holding Pattern 2
FSCGCL - Shimbo Crystal Celestite Schedule
FSCGWM - Wollast-O-Matte Fara Shimbo Crystalline Glaze
FSCRGL - GC106 Base for Crystalline Glazes
FSHP1 - Shimbo Crystal Holding Pattern 1
FSHP3 - Shimbo Crystal Holding Pattern 3
FSNM5 - Fa's Number Five
MDDCL - Medalta Decal Firing
PLC6CR - Cone 6 Crystal Glaze Plainsman
PLC6DS - Cone 6 Drop-and-Soak Firing Schedule
QICA - Quartz Inversion Cracking Avoider

"FSCGCL" Firing Schedule

Shimbo Crystal Celestite Schedule

No kiln will be able to achieve one or more of these rates of climb or drop. And, all but very small or thin-walled ware would crack. Fara’s intention is that the degree to which it is possible will determine how well crystals will grow.

Step °C °F Hold Time
1 100°C/hr to 250C  180°F/hr to 482F  0 2:32  
2 250°C/hr to 350C  450°F/hr to 662F  0 2:56  
3 500°C/hr to 1265C  900°F/hr to 2309F  0 4:46  
4 9999°C/hr to 1130C  17998°F/hr to 2066F  10min 4:56  
5 35°C/hr to 1050C  63°F/hr to 1922F  10min 7:24  
Start temperature assumed: 25°C or 75°F
"Fahrenheit degrees" is not the same as "degrees Fahrenheit". A 100° reading on a Fahrenheit thermometer is equal to a 37° reading on a Celcius thermometer. But "100 Fahrenheit degrees of temperature change" is equivalent "55 Celsius degrees of change". That is an important distinction to understand the above temperature conversions.

Related Information

Links

Recipes CELECG - Celestite Crystalline Glaze
Cone 9-10 - Spodumene, talc variant
Recipes FAC5 - Crystal Number Five Glaze
Cone 8-9 - Spodumene, talc variant

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.