1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

YLO-1888D Yellow Iron Oxide

Description: Harcros easy dispersing yellow iron oxide

Formula: FeOOH

Oxide Analysis Formula Tolerance
Fe2O3 88.00% 1.00
LOI 12.00%n/a
Oxide Weight 160.00
Formula Weight 181.82

Notes

Harcros makes two types of yellow iron; Easy Dispersing and Regular. Both are 99.9% minus 325 mesh and have 85%+ Fe2O3. The former consists of five products ranging from light shade YLO-1888D to deep shade YLO-4088D. These products offer closely controlled mass color, tint, and strength combined with easy dispersion properties.

The regular grade consists of six products from light yellow YO-2087 to deep yellow YO-8087 (density increases and surface area decreases dramatically across this range).

The Hegman values of the regular material are not as high. The products will withstand temperatures to 450-500F in most vehicle systems. They are non-fading and non-reactive in weak acids and alkalis. They are ideal as colorants in paints, enamels, concrete, plastic, rubber and paper.

Related Information

Links

Materials Iron Oxide Black
Materials Spanish Red Iron Oxide
Materials Natural Red Iron Oxide
Materials Mapico 1075A Yellow Iron Oxide
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

Data

Density (Specific Gravity) 4.03
pH for dry powder 7.0

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy