Alternate Names: Pigment Yellow 42
Description: Ferric Oxide Hydrate
Formula: FeOOH
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Fe2O3 | 87.00% | 1.00 | |
| H2O | 12.00% | n/a | |
| Oxide Weight | 160.00 | ||
| Formula Weight | 181.82 | ||
Manufacturer using the Martin process.
Typical trace elements ppm: As < 1, Sb < 8, Cd < 1, Cr < 5, Cu < 1, Pb < 3, Hg < 0.1, Ni < 150, Se < .5
| Materials |
YLO-1888D Yellow Iron Oxide
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| % Passing 325 Mesh Wet | .02 |
|---|---|
| Density (Specific Gravity) | 4.1 |
| pH for dry powder | 6.5 |