Alternate Names: F3269
Description: Leadless high alkali low calcia frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.41% | 0.03 | |
| K2O | 7.42% | 0.29 | |
| Na2O | 10.97% | 0.64 | |
| ZnO | 0.97% | 0.04 | |
| B2O3 | 15.06% | 0.79 | |
| Al2O3 | 12.40% | 0.44 | |
| SiO2 | 51.23% | 3.10 | |
| F | 1.50% | 0.29 | |
| Oxide Weight | 363.58 | ||
| Formula Weight | 363.58 | ||
This is a USA pottery frit. Ferro now calls it Frit 3269-2.
Useful for partially fritted gloss tile glazes for cone 06-01. Balanced enough for use alone (if the application can tolerate its high thermal expansion). Like Frit 3110, the high expansion makes it suitable as a crackle glaze (with an addition of 10% kaolin).
Unlike Frit 3110, this has significant B2O3 and Al2O3 and almost no CaO.
| Materials |
Fusion Frit F-225
|
| Materials |
Pemco Frit P-25
|
| Materials |
Hommel Frit 25
|
| Materials |
Ferro Frit 3819
|
| Materials |
Fusion Frit FZ-25
|
| Materials |
General Frit GF-114
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 259
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| URLs |
https://digitalfire.com/4sight/datasheets/ferropotteryfrits2008.pdf
Ferro Pottery Frits 2008 |
| Co-efficient of Linear Expansion | 9.98 |
|---|---|
| Frit Melting Range (C) | 1400-1500F |