Pemco Frit P-25

Alternate Names: Pemco 25, Pemco Frit 25

Description: Leadless alkaline fluorine frit, use for cone 06-02

Oxide Analysis Formula Tolerance
CaO 0.50% 0.03
K2O 5.40% 0.18
Na2O 14.70% 0.76
ZnO 0.70% 0.03
B2O3 16.90% 0.78
Al2O3 12.10% 0.38
SiO2 49.70% 2.65
F 1.80% 0.30
Oxide Weight 326.35
Formula Weight 326.35

Notes

Often used with 10% clay addition for low temperature crackle glazes. Frequently used as a component in partially fritted wall tile glazes.

Related Information

Links

Materials Hommel Frit 25
Materials Fusion Frit F-225
Materials Ferro Frit 3269
Materials General Frit GF-114
Materials Hommel Frit 259
Materials Ferro Frit 3819
Materials Fusion Frit FZ-25
Materials Pemco Frit Pb-106
Materials Pemco Frit P-2D71
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 10.0 x 10-6 (50-450C)
Frit Melting Range (C) 1320-1420F
I.F.P. (celsius) 575C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy