Alternate Names: Frit FZ25
Description: Boro Sodium Frit, Tile Flux
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.50% | 0.03 | |
| K2O | 5.40% | 0.18 | |
| Na2O | 14.70% | 0.76 | |
| ZnO | 0.70% | 0.03 | |
| B2O3 | 16.90% | 0.78 | |
| Al2O3 | 12.10% | 0.38 | |
| SiO2 | 49.70% | 2.65 | |
| Oxide Weight | 320.58 | ||
| Formula Weight | 320.58 | ||
| Materials |
Ferro Frit 3269
|
| Materials |
General Frit GF-114
|
| Materials |
Pemco Frit P-25
|
| Materials |
Ferro Frit 3819
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 259
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 5.84 |
|---|---|
| Frit Softening Point | 790C |