1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Dead-burned Dolomite

Alternate Names: Calcined Dolomite

Formula: CaO.MgO

Oxide Analysis Formula Tolerance
CaO 58.20% 0.50
MgO 41.80% 0.50
Oxide Weight 48.20
Formula Weight 48.20

Notes

Calcined dolomite is produced by heating raw dolomite, CaMg(CO₃)₂, to drive off carbon dioxide. Complete calcination produces a mixture of calcium oxide (CaO) and magnesium oxide (MgO), commonly called dolime or dolomitic quicklime. Unlike raw dolomite, this material contains free oxides rather than carbonate minerals.

The degree of firing determines its properties. Soft-burned dolomite is relatively porous and reactive. Dead-burned dolomite is fired more intensely to sinter the oxides into dense, less reactive grains suitable for refractory manufacture. Refractory-grade material is commonly called doloma. It is used in bricks and granular repair materials for steelmaking vessels, ladles and certain cement-kiln linings.

Doloma refractories are useful because their CaO and MgO withstand high temperatures and are compatible with suitably controlled basic slags. Dolomitic lime is also added separately to steelmaking slags to adjust their chemistry. Bringing the slag toward MgO saturation reduces its tendency to dissolve MgO from the refractory lining. For doloma linings, the slag’s relationship to CaO saturation also matters. Protection depends on slag composition and operating temperature, rather than simply on the presence of suspended MgO particles.

Like quicklime, calcined dolomite is moisture-sensitive, especially because its free CaO reacts with water to form calcium hydroxide. Dead-burning reduces this reactivity but does not eliminate the need for dry storage. It should not be treated as a direct substitute for raw dolomite in water-based pottery glazes.

For calculation purposes, completely calcined pure dolomite contains approximately 58.2% CaO and 41.8% MgO by weight. Commercial products can differ because of impurities, incomplete calcination or subsequent hydration and carbonation.

Related Information

Links

Materials Dolomite
An inexpensive source of MgO and CaO for ceramic glazes, also a highly refractory material when fired in the absence of reactant fluxes.
Materials Quicklime
Made by heating limestone sufficiently to drive off carbon dioxide. The only ceramic use is the production of refractories (because of its high melting point).
Materials Boric Oxide
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Typecodes Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service.
Glossary Calcination
Calcining is simply firing a ceramic material to create a powder of new physical properties. Often it is done to kill the plasticity or burn away the hydrates, carbonates, sulfates of a clay or refractory material.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved