| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 1.20% | 0.15 | |
| MgO | 0.80% | 0.14 | |
| K2O | 7.00% | 0.54 | |
| Na2O | 1.40% | 0.16 | |
| TiO2 | 0.28% | 0.03 | |
| Al2O3 | 16.00% | 1.14 | |
| SiO2 | 71.00% | 8.55 | |
| Fe2O3 | 0.70% | 0.03 | |
| LOI | 1.50% | n/a | |
| SO3 | 0.10% | n/a | |
| Oxide Weight | 712.22 | ||
| Formula Weight | 723.80 | ||
Aplite A/3 is extracted from an open pit terraced mine in the metal-bearing Tuscany hills. The production process extends from the quarry to the plant, where the material is crushed and reduced to the mercantile grain sizes.
Aplite is used almost exclusively as a flux in single-fired ceramic tile production. It is a unique product in that it contains almost all the components of the ceramic mix: the clay fraction, sodium and potassium feldspars, and quartz. It has a wider sintering range than pure sodium feldspar. In a trend towards shorter and shorter firing times, this property facilitates degassing of the mixture. The Italian market for single-fired ceramics has witnessed a consolidation in the use of aplite in production for its advantages regarding the quality of the finished products.
| Minerals |
Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO |
| Minerals |
K-Feldspar
Most common feldspars contain both sodium and potassium. The term K-Feldspar designates one where th |
| Minerals |
Na-Feldspar
Most common feldspars contain both sodium and potassium. The term Na-Feldspar designates one where t |
| Minerals |
Aplite
An intrusive rock in which quartz and feldspar are the dominant minerals. |
| Typecodes |
Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate. |
| Bulk Density g/cc (Packed) | 1.4 |
|---|---|
| Hardness (Moh) | 6.5 |
| Ultimate Particle Size Distribution | 0-6mm |
| Density (Specific Gravity) | 2.6 |
| pH for dry powder | 8-9 |