Instructions for application:
-Trim around decal.
-Place in shallow pan of warm water, let it curl up. After about 30 seconds it should begin to uncurl, loosen and slide off the paper.
-Position the decal face up and slide it off onto the fired ware surface.
-Sponge from the center until all the excess water, wringles and air bubbles have been removed.
-Let dry for 12-24 hours before firing.
| Step | °C | °F | Hold | Time | |
|---|---|---|---|---|---|
| 1 | 111°C/hr to 43C | 200°F/hr to 110F | 30min | 0:40 | |
| 2 | 111°C/hr to 97C | 200°F/hr to 208F | 45min | 1:54 | |
| 3 | 194°C/hr to 482C | 350°F/hr to 900F | 3:53 | ||
| 4 | 388°C/hr to 821C | 700°F/hr to 1510F | 20min | 5:05 |