Fusion Frit FZ-30

Alternate Names: Fusion Frit FZ30

Description: Zinc barium artware, tile, sanitaryware glaze frit

Oxide Analysis Formula Tolerance
K2O 4.00% 0.11
Na2O 1.40% 0.06
BaO 8.50% 0.14
SrO 7.50% 0.19
ZnO 16.00% 0.50
Al2O3 1.00% 0.03
B2O3 11.50% 0.42
SiO2 39.60% 1.69
ZrO2 10.50% 0.22
Oxide Weight 256.78
Formula Weight 256.78

Related Information

Links

Materials Ferro Frit 3240
Materials Hommel Frit G-26
Materials Pemco Frit P-64
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 69
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.47 x 10-6
Frit Softening Point 1550F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy