Colloid 211

Description: DEFLOCCULANT, DISPERSANT

Notes

Colloid 211 is a neutralized low molecular weight polyacrylate dispersant for pigments in water based systems. It acts to disperse high solids, stabilize viscosity over a wide range of temperatures, control rheology over a broad range of pH and temperature.

Appearance: Clear, Light Amber Liquid
Nonvolatile Matter (NVM) 43%
(NVM = 1/2 gram sample @130 degrees for 1/2 hour)
pH 7-8
Viscosity (Brookfield #2 Spindle @ 30 RPM @ 77 degrees F: 250 cps
SG @ 77F: 1.3
Molecular Weight (Mw-GPC) 3500
Solubility: Water soluble

Application: Use .05-.5% (dry basis) by weight of pigment, depending on system. Colloid 211 is exceptionally effective in clay, calcium carbonate and other pigments, as well as in coatings formulations containing these.

Colloid 211 meets the food additives requirements of CFR 21, sections 173.210 (boiler water), 175.105 (adhesives), 175.300 (coatings), 175.320
(polyolefinfilm), 176.170 (paper and paperboard, aqueous and fatty foods), 176.180 (paper and paperboard - dry foods).

Colloid 211 can be stored over a wide range of temperatures and is not affect by freeze-thaw cycling. Should the product freeze under severe conditions, warm to 40C and mix well before using.

Colloid 211 complies with the Toxic Substances Control Act PL 94-469.
CAS Number 9003-04-7.

Colloids, Inc., 394 Frelinghuysen Ave, Newark, NJ 07114
Colloids Canada Inc, P.O. Box 160, St. Catherines, Ont. L2R 6S4

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Additives for Ceramic Glazes
Materials that are added to glazes to impart physical working properties and usually burn away during firing. In industry all glazes, inks and engobes have additives, they are considered essential to control of cohesion, adhesion, suspension, dry hardness, surface leveling, rheology, speed-of-drying, etc. Among potters, it is common for glazes to have zero additives.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy