Description: Cuban clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 64.80% | 4.69 | |
| Al2O3 | 23.45% | 1.00 | |
| Fe2O3 | 0.42% | 0.01 | |
| TiO2 | 0.65% | 0.04 | |
| CaO | 0.39% | 0.03 | |
| MgO | 0.63% | 0.07 | |
| K2O | 2.07% | 0.10 | |
| Na2O | 0.37% | 0.03 | |
| LOI | 6.44% | n/a | |
| Oxide Weight | 403.56 | ||
| Formula Weight | 431.34 | ||
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
| Materials |
Caolín Gris (Cuba)
|
| Materials |
Caolín Blanco (Cuba)
|
| Materials |
Caolín Mantua (Cuba)
|
| Materials |
Caolín Damanueco (Cuba)
|
| Materials |
Caolín Santa Elena (Cuba)
|
| Materials |
Arcilla Revolucion I (Cuba)
|
| Materials |
Arcilla Revolucion II (Cuba)
|
| Materials |
Arcilla Revolucion III (Cuba)
|
| Materials |
Arcilla Club de Cazadores (Cuba)
|
| Materials |
Barro Ovas (Cuba)
|
| Materials |
Ciego de Avila (Cuba)
|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk