Arcilla Revolucion I (Cuba)

Description: Cuban clay

Oxide Analysis Formula Tolerance
SiO2 52.24% 3.11
Al2O3 28.50% 1.00
Fe2O3 1.96% 0.04
TiO2 0.26% 0.01
CaO 1.11% 0.07
MgO 1.16% 0.10
K2O 1.55% 0.06
Na2O 0.80% 0.05
LOI 10.35%n/a
Oxide Weight 313.44
Formula Weight 349.63

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Materials Arcilla de Pontezuelo (Cuba)
Materials Arcilla Revolucion II (Cuba)
Materials Arcilla Revolucion III (Cuba)
Materials Arcilla Club de Cazadores (Cuba)
Materials Barro Ovas (Cuba)
Materials Ciego de Avila (Cuba)

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy