Alternate Names: Kaolen 113
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.20% | 0.02 | |
| MgO | 0.07% | 0.01 | |
| K2O | 0.04% | - | |
| Na2O | 0.09% | 0.01 | |
| TiO2 | 0.33% | 0.02 | |
| Al2O3 | 21.31% | 1.00 | |
| SiO2 | 70.24% | 5.59 | |
| Fe2O3 | 0.48% | 0.01 | |
| LOI | 7.24% | n/a | |
| SO4 | 0.52% | n/a | |
| Oxide Weight | 443.99 | ||
| Formula Weight | 481.35 | ||
Available in run-of-mine, 25mm and 50mm sizes.
| Minerals |
Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO |
| Minerals |
Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How |
| Materials |
Kaolin 111
|
| Materials |
Kaolin 151
|
| Materials |
Kaolin 115
|
| Materials |
Kaolin 171
|
| Materials |
Kaolin 143
|
| Materials |
Kaolin 114
|
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| Firing Shrinkage | 1000C: 7.3% 1100C: 7.5% 1200C: 7.8% 1250C: 7.9% |
|---|---|
| Water absorption | 1000C: 19.3% 1100C: 18.3% 1200C: 17.5% 1250C: 17% |