I think there is new hope. I have been messaging hundreds of people for days saying this is not about bashing Plainsman, it is about keeping Digitalfire free. Please cool it and wait.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Feldspar 635

Alternate Names: Feldspat 635

Oxide Analysis Formula Tolerance
CaO 0.79% 0.09
MgO 0.34% 0.05
K2O 0.32% 0.02
Na2O 8.62% 0.84
TiO2 0.13% 0.01
Al2O3 16.30% 0.97
SiO2 72.84% 7.35
Fe2O3 0.11% -
LOI 0.55%n/a
Oxide Weight 602.92
Formula Weight 606.25

Notes

Available in 10, 25 and 50mm sizes.

Related Information

Links

Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO
Minerals K-Feldspar
Most common feldspars contain both sodium and potassium. The term K-Feldspar designates one where th
Minerals Na-Feldspar
Most common feldspars contain both sodium and potassium. The term Na-Feldspar designates one where t
Minerals Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How
Materials Feldspar 632
Materials Feldspar 645
Materials Feldspar 661
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy