May 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
Alternate Names: Anhydrous Boric Acid, B2O3
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| B2O3 | 100.00% | 1.00 | |
| Oxide Weight | 69.60 | ||
| Formula Weight | 69.60 | ||
A hard glassy material, granular in texture. Exposed to the atmosphere it slowly absorbs water, reverting to boric acid. It is soluble in water but at a much slower rate than boric acid. Approximately 56.3 kg of boric oxide are the chemical equivalent of 100 kg of boric acid. Boric oxide is used where B2O3 is required without the presence of sodium or calcium and/or where water would be detrimental to the process.
Specialty ceramics: Boric oxide is used to produce various types of high strength and heat-resistant ceramic products such as boron carbide, boron nitride, titanium and zirconium diborides, as well as elemental boron.
Refractories: It is used in the manufacture of chemically bonded firebricks and castables which require resistance to high temperature, abrasion and corrosion. Boric oxide is used as a binder for magnesia-based refractory bricks and as a stabilizer for dolomite refractory bricks commonly used in steel smelting furnaces.
Glazes, frits and enamels: Suppliers speak of boric oxide as increasing strength, scratch resistance, and chemical resistance of ceramic wares such as wall and floor tiles, tableware and porcelain and of enameled appliances, however they do not say compared to what.
| URLs |
http://www.borax.com/pdfs/dist/Profile_Boric_Oxide.pdf
Boric Oxide Data Sheet |
| Materials |
Anhydrous Borax
A white, odorless product crystalline granular by dehydrating Borax to remove the crystal bound water. |
| Materials |
Borax Pentahydrate
|
| Materials |
Borax Decahydrate
|
| Materials |
Boric Acid
|
| Materials |
Calcined Dolomite
|
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| Oxides | B2O3 - Boric Oxide |
| Minerals |
Borate Minerals
The major borate minerals are Colemanite and Ulexite. The geology required for borates is found in v |
| Decomposition Temperature | 185C |
|---|---|
| Frit Softening Point | 577C |
| Density (Specific Gravity) | 1.5-1.75 |