Pyrofrac

Description: Pyrophyllite/Andalusite

Oxide Analysis Formula Tolerance
K2O 0.20% 0.01
Na2O 0.20% 0.02
TiO2 0.40% 0.03
Al2O3 16.50% 1.00
SiO2 76.90% 7.91
Fe2O3 1.00% 0.04
LOI 4.80%n/a
Oxide Weight 588.51
Formula Weight 618.18

Notes

The Pyrofrac group of mineral products is composed of co-products from the Andafrac series. These are smaller grain derivatives of coarser beneficiated Andalusite/Pyrophyllite ores. The broad range of alumina contents in this series enables tuning to a specific application. Some of these products have proven effective as components in refractory mixes, industrial ceramic products, coatings for the structural clay industry.

This analysis is for the 0204 grade which is representative of the many grades available.
The various grades differ in particle size from a coarse grog to fine powder. Alumina content varies from 13.5 to 21.0, alkalies from 0.4 to 0.9, LOI from 3.0 to 5.7.

Related Information

Links

Materials Alkatrol
Materials Andafrac
Materials Pyrotrol
Materials Pyrophyl
Materials Sericite Y/T
A commercial grade of sericite mineral.
Materials Andalusite
A low expansion aluminum silicate mineral that converts to mullite on repeated firings.
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Materials Pyrofrac 0204
Materials Pyrofrac 0304
Materials Pyrofrac 1655
Materials Pyrofrac 1004
Materials Pyrofrac 1855
Materials Pyrofrac 2024
Materials Pyrofrac 2034
Materials Pyrofrac 4203
Materials Pyrofrac 4205
Materials Pyrofrac 2023
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

Data

Pyrometric Cone Equivalent 23-29
Density (Specific Gravity) 2.6-2.7

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy