Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pyrofrac 4205

Oxide Analysis Formula Tolerance
K2O 0.20% 0.02
Na2O 0.20% 0.03
TiO2 0.40% 0.04
Al2O3 12.00% 1.00
SiO2 82.80% 11.71
Fe2O3 1.00% 0.05
SO4 3.00%n/a
H2O 3.40%n/a
Oxide Weight 821.10
Formula Weight 877.24

Notes

Used in structural clay coatings, refractory formulations, whiteware ceramics, art pottery to
increase refractoriness, reduce shrinkage, and widen firing range.
This material is made by crushing & screening of selectively mined andalusite/pyrophyllite/sericite ores
with heavy media separation.

Related Information

Links

Materials Andalusite
A low expansion aluminum silicate mineral that converts to mullite on repeated firings.
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Materials Alkatrol
Materials Pyrofrac

Data

Bulk Density lbs/cu. ft. (Packed) 105
Pyrometric Cone Equivalent 23
Sieve Analysis Dry +20 mesh: 5.0 +50 mesh: 90.0 +70 mesh: 5.0
Density (Specific Gravity) 2.6

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved