This happens in stages: MnO2 to Mn2O3 to Mn3O4 and finally to MnO. The LOI is 18%.

This picture has its own page with more detail, click here to see it.
These metal oxides have been mixed with 50% Ferro frit 3134 and fired to cone 6 oxidation. Chrome and rutile have not melted, copper and cobalt are extremely active melters, frothing and boiling. Cobalt and copper have crystallized during cooling. Manganese has formed an iridescent glass.
| Materials |
Manganese Dioxide
A source of MnO used in ceramic glazes and the production of ceramic stains. Commonly made by grinding pyrolusite rock. |
| Temperatures | Manganese compounds may begin to fume (932-) |
| URLs |
https://fscimage.fishersci.com/msds/13610.htm
Fisher Scientific MnO2 SDS |
| URLs |
https://www.sciencedirect.com/science/article/abs/pii/S0925838823025112#:~:text=Manganese%2520dioxide%2520(MnO2)%2520undergo,reaching%2520to%25201200%2520%C2%B0C.
The decomposition of MnO2. |