All Temperature Numbers Temperature Listing
Loses 28% weight as it decomposes to to the heat stable CuO
| Materials |
Copper Carbonate Basic
This form of copper carbonate is the article of commerce, a mixture of theoretical copper carbonate and copper hydroxide. |
| Temperatures | Decarbonation (200-1000) |
| Glossary |
Carbon Burnout
Ceramic materials, especially clays, often contain carbon and organic compounds. When they are fired in a kiln, these must burn out, often producing complications. |