50-250C | 80C-250C | 120C | 150C | 180C | 185C | | 200C-1000C | 200C-450C | 210C-280C | 250C-370C | 260C | 290C | 300C | 300C-330C | 370-950C | 400C | 425C-650C | 480C-600C | 500C-600C | 512C | 535C | 540C-600C | 650C-900C | 700F | 750C-1000C | 750-850 | 800C-1100C | 850-950 | 850C+ | 850C | 900C | 900-1000 | 990C | 1025-1325 | 1025C+ | 1050C | 1082C | 1100C+ | 1100C | 1300C | 1325C | 1330C | 1360C | 1400F | 1400F | 1418C-1428C | 1420C | 1500F | 1550C | 1565C | 1600F-1650F | 1650F | 1785C | 1800F | 1950F-2050F | 1990C | 2300C | 2320C | 2750F

200C

Manganese Carbonate decomposes to MnO

Release of carbon dioxide to give manganese(II) oxide:

MnCO3 -> MnO + CO2

Related Information

Links

Materials Manganese Carbonate
Temperatures Decarbonation (200C-1000C)
Glossary Carbon Burnout
Ceramic materials, especially clays, often contain carbon and organic compounds. When they are fired in a kiln, these must burn out, often producing complications.

By Tony Hansen


Tell Us How to Improve This Page

Version: Oct/2020

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture

Please check recaptcha to proceed


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved