Description: White Sodium Bentonite
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 1.89% | 0.21 | |
| K2O | 1.06% | 0.07 | |
| MgO | 3.44% | 0.54 | |
| Na2O | 1.65% | 0.17 | |
| TiO2 | 1.47% | 0.12 | |
| Al2O3 | 13.00% | 0.81 | |
| SiO2 | 70.10% | 7.43 | |
| Fe2O3 | 1.45% | 0.06 | |
| LOI | 5.90% | n/a | |
| Oxide Weight | 599.43 | ||
| Formula Weight | 637.02 | ||
A highly purified, white, sodium bentonite supplied as a free-flowing powder. Used when high purity and high whiteness are important in suspending glazes.
Specific Gravity: 2.5
pH (5% dispersion): 9.0-10.0
C.E.C. (meq/100g): 70
Dry Brightness (Green Filter): 87
Color: White
% Moisture Content: 10% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 1098cps
| Materials |
Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying. |
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk