Soft Wood Ash

Alternate Names: Softwood Ash

Description: Washed

Oxide Analysis Formula Tolerance
CaO 41.10% 0.67
K2O 10.96% 0.11
MgO 8.21% 0.19
Na2O 0.77% 0.01
P2O5 4.67% 0.03
SiO2 2.00% 0.03
Fe2O3 0.07% -
MnO 2.54% 0.03
LOI 23.00%n/a
SO3 6.69%n/a
Oxide Weight 64.04
Formula Weight 91.09

Related Information

Links

Materials Cherry Ash
A type of wood ash used as an ingredient in pottery glazes.
Materials Hardwood Ash
A type of wood ash used as an ingredient in pottery glazes.
Materials Eucalyptus Ash
A type of wood ash used as an ingredient in pottery glazes.
Materials Oakwood Ash
A type of wood ash used as an ingredient in pottery glazes.
Materials Applewood Ash
A type of wood ash used as an ingredient in pottery glazes.
Materials Wood Ash
For centuries, pottery glazes have been made from ash mostly mixed with clay and feldspar.
Materials Pine Wood Ash
A type of wood ash used as an ingredient in pottery glazes.
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Glossary Wood Ash Glaze
Common washed wood ash can supply important ceramic oxides when melted, so it can comprise significant percentages in a recipe. Plus it can produce unique visual effects.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy