Description: Plainsman native refractory ball clay

Oxide Analysis Formula Tolerance
BaO 0.20% 0.01
CaO 0.30% 0.03
K2O 0.90% 0.05
TiO2 0.70% 0.05
Al2O3 19.30% 1.00
SiO2 66.00% 5.80
Fe2O3 1.80% 0.06
MnO 0.04% -
MgO 0.50% 0.07
LOI 10.30%n/a
Oxide Weight 474.27
Formula Weight 528.73

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.
Materials Plainsman Fireclay

Data

Frit Softening Point PCE 27

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy