Noor Talc

Alternate Names: One Talc, Egyptian Talc

Description: Talc

Oxide Analysis Formula Tolerance
CaO 0.30% 0.01
MgO 30.48% 0.99
Na2O 0.02% -
Al2O3 1.65% 0.02
SiO2 60.10% 1.31
Fe2O3 0.45% -
LOI 6.98%n/a
H2O 0.55%n/a
Oxide Weight 122.05
Formula Weight 131.99

Related Information

Links

Materials Talc
A source of MgO for ceramic glazes, a flux or thermal expansion additive in clay bodies, also used in the manufacture of cordierite.
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Hazards Talc Hazards Overview
Talc is invaluable in the ceramics industry, it is used as a glaze and body ingredient and as a parting a release agent in various processes. Is it safe?