Ferro Frit 3403

Description: Lead alumina bisilicate frit

Oxide Analysis Formula Tolerance
CaO 0.10% 0.01
K2O 1.40% 0.05
Na2O 0.30% 0.01
PbO 67.80% 0.93
Al2O3 2.30% 0.07
SiO2 28.10% 1.44
Oxide Weight 307.46
Formula Weight 307.46

Notes

Cone Range: 08-02
This is basically a lead bisilicate frit with a few impurities.
Very low melting temperature.

Related Information

Links

Materials Fusion Frit FL-42
Materials Pemco Frit Pb-723
Materials General Frit GF-9
Materials Ferro Frit 3602
A lead bisilicate frit with 2.5% alumina oxide.
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 437
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.2
Frit Melting Range (C) 1350F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy