1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit Pb-723

Alternate Names: Frit Pb723

Description: Soda-lead-alumina-silicate low melting glaze frit

Oxide Analysis Formula Tolerance
Na2O 1.50% 0.07
PbO 71.20% 0.93
Al2O3 2.40% 0.07
SiO2 24.90% 1.21
Oxide Weight 291.38
Formula Weight 291.38

Related Information

Links

Materials General Frit GF-9
Materials Ferro Frit 3403
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 437
Materials Hommel Frit 71
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.00
Co-efficient of Linear Expansion 9.0 x 10-6 (40-450C)
Frit Softening Point 1150F
Frit Melting Range (C) 1100-1250F
I.F.P. (celsius) 490C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy