Ceraflux

Alternate Names: Frit B-300

Description: Lead alumina bilsilicate frit

Oxide Analysis Formula Tolerance
PbO 65.00% 1.00
Al2O3 3.00% 0.10
SiO2 32.00% 1.83
Oxide Weight 343.38
Formula Weight 343.38

Notes

Raw color: Very light yellow
Form: Granular or finely ground frit
Specific Gravity: 4.6 g/cm3
Density, lbs/cu ft, Granlar: 155-175; Ground: 135-155
Melting Range: 788-816C
COE: 7.1 x 10-6

The powdered material is ~2% +200 mesh.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3626
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Materials Lead Bisilcate B-15
Materials BPS Lead Bisilicate
Materials Ferro Frit 3489
Materials Ceraflux
Materials Frit 3647
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs https://hammondglobal.com/wp-content/uploads/2022/06/Ceraflux-0512.pdf
Hammond Lead Products Ceraflux lead bisilicate data sheet
Specially formulated for use in pottery and wall-tile glazes. Lead bisilicate is extremely resistant to leaching by dilute acids, including gastric juices, which reduces its toxicity and offers the maximum safety of any of the lead products. Available in either granulated or ground form.

Data

Frit Softening Point 800C
Frit Softening Point 788-816C
Density (Specific Gravity) 4.50
Density (Specific Gravity) 4.55-4.7

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy