Frit 3647

Description: Lead bilsilicate frit

Oxide Analysis Formula Tolerance
Al2O3 1.48% 0.05
SiO2 33.56% 1.92
PbO 64.96% 1.00
Oxide Weight 343.60
Formula Weight 343.60

Notes

Lead bisilicate with 1.5% Al2O3. Used in Europe.

Related Information

Links

Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Materials Ceraflux
An alumina lead bisilicate from Hammond Lead Products in Indiana. The data sheet claims it is safe and insoluble in stomach acid.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy