Description: Lead alumina bilsilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 64.97% | 1.00 | |
| Al2O3 | 2.67% | 0.09 | |
| SiO2 | 32.36% | 1.85 | |
| Oxide Weight | 343.54 | ||
| Formula Weight | 343.54 | ||
| Materials |
Ferro Frit 3626
|
| Materials |
Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable. |
| Materials |
Ceraflux
An alumina lead bisilicate from Hammond Lead Products in Indiana. The data sheet claims it is safe and insoluble in stomach acid. |
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |