Bonding Clay

Description: Cedar Heights Bonding

Oxide Analysis Formula Tolerance
CaO 0.20% 0.01
K2O 1.70% 0.06
MgO 0.30% 0.03
Na2O 0.20% 0.01
TiO2 1.60% 0.07
Al2O3 29.40% 1.00
SiO2 54.70% 3.16
Fe2O3 1.70% 0.04
LOI 10.10%n/a
Oxide Weight 311.55
Formula Weight 346.55

Notes

AVailable in 12/30/200 mesh sizes.
A light buff burning fireclay.

Related Information

Fired bars of Cedar Heights Bonding clay


This picture has its own page with more detail, click here to see it.

They are fired from cone 4 to 10 oxidation (top down) and cone 10 reduction (bottom).

Links

Materials Goldart
A plastic buff burning clay, often used as a major ingredient in stoneware clay bodies.
Materials Industrial Fireclay
Materials CKR Clay
Materials Fireclay A/S
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

Data

Pyrometric Cone Equivalent 31

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy