Description: Alkaline borate bonding frit for abrasive industry
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 10.70% | 0.52 | |
| K2O | 2.60% | 0.07 | |
| Na2O | 9.30% | 0.41 | |
| B2O3 | 15.60% | 0.61 | |
| Al2O3 | 7.81% | 0.21 | |
| SiO2 | 54.00% | 2.44 | |
| Oxide Weight | 271.52 | ||
| Formula Weight | 271.52 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Fusion Frit F-34
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Typecodes |
Bonding Frits
Also called glass frits, these melt at very low temperatures (e.g. 500C). They are used to bond together materials that can withstand some heat (e.g. abrasives, ceramics, non-oxide ceramics, metals). And as a surface-smoothing agent. The main product properties are melting temperature and thermal expansion. The powders are mixed with binders, applied and then heated up and down to create the bond. |