Alternate Names: Fusion Frit F34
Description: High boron zinc free calcium frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 12.00% | 0.51 | |
| Na2O | 12.50% | 0.49 | |
| B2O3 | 27.50% | 0.95 | |
| SiO2 | 48.00% | 1.92 | |
| Oxide Weight | 240.66 | ||
| Formula Weight | 240.66 | ||
| Materials |
Ferro Frit 3191
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 3193
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.43 x 10-6 |
|---|---|
| Frit Softening Point | 1600F |