Gelwhite H

Description: Highly refined bentonite plasticizer

Notes

A very white burning highly processed montmorillonite material (similar to Mineral Colloid BP from the same company, Southern Clay Products). Although this material is targeted at the cosmetics industry, it can be useful in ceramics as a white burning plasticizer. These materials are almost equal to Veegum for use in producing very white burning plastic porcelains.

Was made by Southern Clay products but discontinued by new owners.

Related Information

Mineral Colloid BP, Gelwhite H, Veegum T in plastic form


This picture has its own page with more detail, click here to see it.

Each has been mixed with water and all produce a jelly-like translucent sticky material that takes a very very long time to dry. They are expensive and, among other uses, act as white-burning plasticizers in fine porcelain bodies.

Veegum T , Mineral Colloid BP, Gelwhite H at cone 6


This picture has its own page with more detail, click here to see it.

The Veegum is dense and white, but not melting. The Mineral Colloid fires like a typical raw bentonite (dark brown, high soluble salts and beginning to melt). The Gelwhite is completely melted and foamed.

Links

Oxide Analysis Formula Tolerance
Materials Mineral Colloid BP
Materials Veegum
A clay of incredibly small particle size. It has the highest plasticity of any known clay and acts as a suspending and gelling agent in slurries.
Minerals Montmorillonite, Bentonite
A clay mineral of extremely small particle size and high plasticity. Raw bentonite is generally a pa

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy