Description: Washed
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 20.26% | 0.37 | |
| K2O | 10.33% | 0.11 | |
| MgO | 11.94% | 0.31 | |
| Na2O | 10.83% | 0.18 | |
| Al2O3 | 2.21% | 0.02 | |
| P2O5 | 3.41% | 0.02 | |
| SiO2 | 32.90% | 0.57 | |
| Fe2O3 | 3.50% | 0.02 | |
| MnO | 0.51% | 0.01 | |
| SO3 | 4.11% | n/a | |
| Oxide Weight | 99.29 | ||
| Formula Weight | 103.54 | ||
| Materials |
Cherry Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Applewood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Hardwood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Oakwood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Pine Wood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Rice Husk Ash
A type of plant ash used as an ingredient in pottery glazes. |
| Materials |
Rice Straw Ash
A type of plant ash sometimes used as an ingredient in pottery glazes. |
| Materials |
Soft Wood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Wood Ash
For centuries, pottery glazes have been made from ash mostly mixed with clay and feldspar. |
| Hazards |
Plant Ash Toxicity
The hazards of using plant and wood ash in ceramic glazes |
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| Glossary |
Wood Ash Glaze
Common washed wood ash can supply important ceramic oxides when melted, so it can comprise significant percentages in a recipe. Plus it can produce unique visual effects. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk