Description: Pyrophyllite
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 0.20% | 0.01 | |
| Na2O | 0.20% | 0.01 | |
| TiO2 | 0.40% | 0.02 | |
| Al2O3 | 22.30% | 1.00 | |
| SiO2 | 73.30% | 5.58 | |
| Fe2O3 | 0.70% | 0.02 | |
| LOI | 2.80% | n/a | |
| Oxide Weight | 444.13 | ||
| Formula Weight | 456.93 | ||
The PYROPHYL group of mineral products consists of milled co-products of the Andafrac series and various milled combinations of the Pyrofrac and Andafrac series. The broad range of alumina contents allows for both whiteware and refractory applications.
Pyrophyl is a high melting material and is used to reduce hot load deformation and improve volume stability in refractories. It is used in foundry mold and core wash formulations, technical ceramics, structural clay coatings, art pottery.
This material is dry milled and magnetically separated.
The analysis shown here is an average.
| Materials |
Alkatrol
|
| Materials |
Andafrac
|
| Materials |
Pyrofrac
|
| Materials |
Pyrotrol
|
| Materials |
Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc. |
| Materials |
Sericite Y/T
A commercial grade of sericite mineral. |
| Materials |
Pyrophyl R-1403
|
| Materials |
Pyrophyl R-1404
|
| Materials |
Pyrophyl R-2252
|
| Materials |
Pyrophyl R-2253
|
| Materials |
Pyrax Pyrophyllite
|
| Typecodes |
Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate. |
| Bulk Density lbs/cu. ft. (Packed) | 55-70 |
|---|---|
| Pyrometric Cone Equivalent | 26-29 |
| Sieve Analysis Dry | +200 mesh: 1-12% |
| Density (Specific Gravity) | 2.7-2.75 |