Fireclay A/S

Oxide Analysis Formula Tolerance
CaO 0.20% 0.01
MgO 0.50% 0.05
K2O 2.30% 0.10
Na2O 0.10% 0.01
TiO2 1.50% 0.08
Al2O3 25.40% 1.00
SiO2 60.90% 4.07
Fe2O3 1.60% 0.04
LOI 7.50%n/a
Oxide Weight 371.46
Formula Weight 401.57

Notes

Dark buff burning fireclay available in 12 or 30 mesh.

Related Information

Links

Materials Goldart
A plastic buff burning clay, often used as a major ingredient in stoneware clay bodies.
Materials Ceramic Fireclay
'Ceramic Fireclay' is a trade name for a clay from Resco Products.
Materials Bonding Clay
Materials Fireclay
Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

Data

Pyrometric Cone Equivalent 27

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy