Ceramic Fireclay

Oxide Analysis Formula Tolerance
Na2O 0.20% 0.01
K2O 1.90% 0.07
CaO 0.20% 0.01
MgO 0.40% 0.04
TiO2 1.80% 0.08
Fe2O3 1.40% 0.03
SiO2 55.20% 3.25
Al2O3 28.80% 1.00
LOI 10.00%n/a
Oxide Weight 318.40
Formula Weight 353.77

Notes

'Ceramic Fireclay' is a trade name for a clay from Resco Products, not a generic term.

Related Information

Links

Materials Goldart
A plastic buff burning clay, often used as a major ingredient in stoneware clay bodies.
Materials Industrial Fireclay
Materials Fireclay A/S
Materials Roseville Clay
Materials Fireclay
Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

Data

Pyrometric Cone Equivalent 29-31

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy