Alternate Names: Argentinian Hydroborocite
Formula: CaO.MgO.3B2O3.6H2O
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 14.50% | 0.66 | 1.5 |
| MgO | 5.40% | 0.34 | 0.8 |
| B2O3 | 30.00% | 1.10 | Min |
| SiO2 | 12.00% | 0.51 | 2.0 |
| Fe2O3 | 0.55% | 0.01 | 0.15 |
| SO4 | 2.50% | n/a | |
| LOI | 20.00% | n/a | |
| Oxide Weight | 159.12 | ||
| Formula Weight | 205.32 | ||
Also CaMgB6O8(OH)6:3(H2O)
This is mined in North Argentina, in the Andes Mountains, at about 4500 meters altitude. Material is normally sold in bulk bag but the company has facilities to pack in 25 and 50 kg bags also.
As2O3: 300-600 ppm
Size Granulated or Crushed to 20 mesh
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| Minerals |
Hydroboracite
A minor borate ore. |
| Materials |
Chilean Ulexite
|
| Materials |
Turkish Ulexite
A mineral with very high B2O3 and CaO content. |
| Materials |
Ulexite
A natural source of boron, it melts at a very low temperature to a clear glass. |