Cedar Heights Fireclay

Description: Fire Clay

Oxide Analysis Formula Tolerance
CaO 0.57% 0.05
MgO 0.11% 0.01
Na2O 0.50% 0.04
TiO2 0.31% 0.02
Al2O3 22.06% 1.00
SiO2 66.62% 5.13
Fe2O3 1.70% 0.05
LOI 8.13%n/a
Oxide Weight 424.78
Formula Weight 462.38

Notes

A raw clay similar to the more well known Goldart. It is used in the formulation of middle and high temperature stoneware clay bodies. It's non-uniform texture and firing properties make for interesting fired surfaces.

Related Information

Links

Materials Plainsman Fireclay
Materials Fireclay
Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

Data

Pyrometric Cone Equivalent 30

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy