BENTOLITE L10

Oxide Analysis Formula Tolerance
CaO 1.67% 0.24
K2O 0.06% 0.01
MgO 3.65% 0.73
Na2O 0.20% 0.03
TiO2 0.28% 0.03
Al2O3 15.49% 1.22
SiO2 71.99% 9.64
Fe2O3 0.72% 0.04
LOI 5.93%n/a
Oxide Weight 757.32
Formula Weight 805.06

Notes

Aluminum silicate additive for paints and coatings. An economical thixotrope. BENTOLITE L10 contributes to excellent application and film formation properties. In glazes, when used in combination with carboxymethylcellulose, Bentolite provides for improved rheology, solids suspension, glaze adhesion and sprayability.

Related Information

Links

Materials Bentolite L-3
Materials Bentolite H
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy