Texas Talc 92

Alternate Names: TxTalc92

Description: A talc having a rounded rather than platy particle shape.

Oxide Analysis Formula Tolerance
CaO 5.50% 0.13
MgO 26.30% 0.86
K2O 0.40% 0.01
Na2O 0.40% 0.01
Al2O3 0.60% 0.01
SiO2 56.00% 1.22
Fe2O3 0.60% -
LOI 10.10%n/a
Oxide Weight 117.95
Formula Weight 131.20

Related Information

Links

Materials Talc
A source of MgO for ceramic glazes, a flux or thermal expansion additive in clay bodies, also used in the manufacture of cordierite.
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy