Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.24% | 0.01 | |
| K2O | 0.60% | 0.02 | |
| MgO | 0.24% | 0.02 | |
| Na2O | 0.56% | 0.03 | |
| TiO2 | 0.71% | 0.03 | |
| Al2O3 | 35.52% | 1.00 | |
| SiO2 | 45.65% | 2.18 | |
| Fe2O3 | 1.25% | 0.02 | |
| LOI | 15.22% | n/a | |
| Oxide Weight | 243.43 | ||
| Formula Weight | 287.13 | ||
| Materials |
Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries. |
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk