Stain 6336

Description: Peacock Blue (CrCoAlSiSnZn)

Notes

Old Number: 1036

Related Information

Blue stain in a low-fire porcelain:

Creates the blue-white color of reduction-fired bodies


This picture has its own page with more detail, click here to see it.

The top Zero3 porcelain bar has 0.07% Mason 6336 blue stain added (vs. none in the bottom bar). Zero3 is a frit-fluxed body, these SHAB test bars are fired at cone 03 in oxidation. To match the color of a cone 10 reduction clear glazed Grolleg porcelain (e.g. L3778D) I add 0.05% stain blue stain (because the transparent glaze amplifies the color). In either case, to ensure that color develops, the body still must have adequate glass development (which is no problem in a fritware body).

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy