1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Sodium Nitrate

Alternate Names: Chile Saltpeter, Soda Niter

Description: A source of sodium in the glass industry

Formula: NaNO3

Oxide Analysis Formula Tolerance
Na2O 36.47% 1.00
LOI 63.53%n/a
Oxide Weight 62.00
Formula Weight 170.00

Related Information

Links

URLs http://en.wikipedia.org/wiki/Sodium_nitrate
Sodium Nitrate at Wikipedia
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Materials Sodium Carbonate
Materials Anhydrous Sodium Sulfate

Data

Frit Softening Point 310C
Density (Specific Gravity) 2.27

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy