Anhydrous Sodium Sulfate

Alternate Names: Salt Cake, Sodium Sulphate

Description: A source of sodium in the glass industry

Formula: Na2SO4

Oxide Analysis Formula Tolerance
Na2O 43.70% 1.00
SO3 56.30%n/a
Oxide Weight 62.00
Formula Weight 141.88

Related Information

Links

Materials Sodium Sulfate Decahydrate
Materials Sodium Nitrate
Hazards Sulfur Dioxide Toxicity
This gas can be produced when clays are fired in a kiln. What can you do?
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy