Sodium Hexametaphosphate

Alternate Names: SHMP, Calgon

Description: Deflocculant

Formula: (NaPO3)6

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Tetrasodium Pyrophosphate
Typecodes Additives for Ceramic Glazes
Materials that are added to glazes to impart physical working properties and usually burn away during firing. In industry all glazes, inks and engobes have additives, they are considered essential to control of cohesion, adhesion, suspension, dry hardness, surface leveling, rheology, speed-of-drying, etc. Among potters, it is common for glazes to have zero additives.
URLs http://en.wikipedia.org/wiki/Sodium_hexametaphosphate
Sodium Hexametaphosphate at Wikipedia

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy