Tetrasodium Pyrophosphate

Description: Powerful deflocculant

Formula: Na4P2O7

Oxide Analysis Formula Tolerance
Na2O 46.62% 0.67
P2O5 53.38% 0.33
Oxide Weight 88.64
Formula Weight 88.64

Related Information

Links

Materials Tetrasodium Pyrophosphate Hydrated
Materials Sodium Hexametaphosphate
Typecodes Additives for Ceramic Glazes
Materials that are added to glazes to impart physical working properties and usually burn away during firing. In industry all glazes, inks and engobes have additives, they are considered essential to control of cohesion, adhesion, suspension, dry hardness, surface leveling, rheology, speed-of-drying, etc. Among potters, it is common for glazes to have zero additives.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy