PotteryCrafts Frit P3124

Alternate Names: PotteryCrafts Frit 3124

Description: This is actually Ferro Frit 3124

Oxide Analysis Formula Tolerance
CaO 14.10% 0.70
K2O 0.70% 0.02
Na2O 6.30% 0.28
B2O3 13.70% 0.55
Al2O3 9.90% 0.27
SiO2 55.30% 2.55
Oxide Weight 277.48
Formula Weight 277.48

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3124
A commonly available calcium borosilicate frit. It is glaze-like, needing only a kaolin addition to create a low-temperature glossy glaze.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.9
Frit Melting Range (C) 1000-1020

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy